Ceramic Ball
Product Number | System of measurement |
Roller Diameter | Material | Hardness | Coefficient Of Thermal Expansion |
Thermal Conductivity | Sphericity | Density | Weight | price | Cart |
---|---|---|---|---|---|---|---|---|---|---|---|
Al2O3-1 inch | Inch | 1" | Alumina(Al2O3) | 80 HRC | 46 × 10-7/° F | 194.5 Btu/hr. × in./sq. ft./°F @ 212° F | 0.000010" | 3.95 g/cm3 | 33.55g | Inquiry |
|
Si3N4-7/64 inch G5 | Inch | 0.109375" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000005" | 3.20~3.30 g/cm3 | 0.03615g | Inquiry |
|
Si3N4-1 inch G5 | Inch | 1" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000005" | 3.20~3.30 g/cm3 | 27.63g | Inquiry |
|
Si3N4-3/4 inch | Inch | 0.75" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000010" | 3.20~3.30 g/cm3 | 11.66g | Inquiry |
|
SiC-15/32 inch | Inch | 0.46875" | Silicon carbide (SIC) | 85~90 HRC | 2.2 x 10–6/°F | 120 W/m-K @ 20° C | 0.000010" | 3.10 g/cm3 | 2.757g | Inquiry |
|
Al2O3-7/64 inch | Inch | 0.109375" | Alumina(Al2O3) | 80 HRC | 46 × 10-7/° F | 194.5 Btu/hr. × in./sq. ft./°F @ 212° F | 0.000010" | 3.95 g/cm3 | 0.04389g | Inquiry |
|
Si3N4-3/32 inch | Inch | 0.09375" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000010" | 3.20~3.30 g/cm3 | 0.02276g | Inquiry |
|
Si3N4-15/16 inch | Inch | 0.9375" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000010" | 3.20~3.30 g/cm3 | 22.77g | Inquiry |
|
SiC-19/32 inch | Inch | 0.59375" | Silicon carbide (SIC) | 85~90 HRC | 2.2 x 10–6/°F | 120 W/m-K @ 20° C | 0.000010" | 3.10 g/cm3 | 5.603g | Inquiry |
|
Al2O3-15/64 inch | Inch | 0.234375" | Alumina(Al2O3) | 80 HRC | 46 × 10-7/° F | 194.5 Btu/hr. × in./sq. ft./°F @ 212° F | 0.000010" | 3.95 g/cm3 | 0.4319g | Inquiry |
|
ZrO2-29/64 inch | Inch | 0.453125" | Zirconia (ZRO2) | 70 HRC | 5.7 x 10–6/°F | 2 W/m-K @ 20° C | 0.000010" | 6.00 g/cm3 | 4.821g | Inquiry |
|
Al2O3-1 3/8 inch | Inch | 1.375" | Alumina(Al2O3) | 80 HRC | 46 × 10-7/° F | 194.5 Btu/hr. × in./sq. ft./°F @ 212° F | 0.000010" | 3.95 g/cm3 | 87.21g | Inquiry |
|
Si3N4-15/64 inch G5 | Inch | 0.234375" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000005" | 3.20~3.30 g/cm3 | 0.3557g | Inquiry |
|
Si3N4-5/4 inch | Inch | 1.25" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000010" | 3.20~3.30 g/cm3 | 53.96g | Inquiry |
|
SiC-3/4 inch | Inch | 0.75" | Silicon carbide (SIC) | 85~90 HRC | 2.2 x 10–6/°F | 120 W/m-K @ 20° C | 0.000010" | 3.10 g/cm3 | 11.29g | Inquiry |
|
Al2O3-11/32 inch | Inch | 0.34375" | Alumina(Al2O3) | 80 HRC | 46 × 10-7/° F | 194.5 Btu/hr. × in./sq. ft./°F @ 212° F | 0.000010" | 3.95 g/cm3 | 1.363g | Inquiry |
|
ZrO2-9/16 inch | Inch | 0.5625" | Zirconia (ZRO2) | 70 HRC | 5.7 x 10–6/°F | 2 W/m-K @ 20° C | 0.000010" | 6.00 g/cm3 | 9.225g | Inquiry |
|
Si3N4-11/32 inch G5 | Inch | 0.34375" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000005" | 3.20~3.30 g/cm3 | 1.122g | Inquiry |
|
Si3N4-7/32 inch | Inch | 0.21875" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000010" | 3.20~3.30 g/cm3 | 0.2892g | Inquiry |
|
Al2O3-29/64 inch | Inch | 0.453125" | Alumina(Al2O3) | 80 HRC | 46 × 10-7/° F | 194.5 Btu/hr. × in./sq. ft./°F @ 212° F | 0.000010" | 3.95 g/cm3 | 3.121g | Inquiry |
|
ZrO2-23/32 inch | Inch | 0.71875" | Zirconia (ZRO2) | 70 HRC | 5.7 x 10–6/°F | 2 W/m-K @ 20° C | 0.000010" | 6.00 g/cm3 | 19.24g | Inquiry |
|
Si3N4-29/64 inch G5 | Inch | 0.453125" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000005" | 3.20~3.30 g/cm3 | 2.57g | Inquiry |
|
Si3N4-5/16 inch | Inch | 0.3125" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000010" | 3.20~3.30 g/cm3 | 0.8433g | Inquiry |
|
SiC-3/32 inch | Inch | 0.09375" | Silicon carbide (SIC) | 85~90 HRC | 2.2 x 10–6/°F | 120 W/m-K @ 20° C | 0.000010" | 3.10 g/cm3 | 0.02205g | Inquiry |
|
Si3N4-1 7/8 inch | Inch | 1.875" | Silicon Nitride (Si3N4) | 75~80 HRC | 15 × 10-7/° F | 29 W/m-K @ 20° C | 0.000010" | 3.20~3.30 g/cm3 | 182.12g | Inquiry |
|
SiC-15/16 inch | Inch | 0.9375" | Silicon carbide (SIC) | 85~90 HRC | 2.2 x 10–6/°F | 120 W/m-K @ 20° C | 0.000010" | 3.10 g/cm3 | 22.06g | Inquiry |
|
-
show / page